Logo image
Effect of milling in oxygen on sphalerite-bearing materials
Journal article   Peer reviewed

Effect of milling in oxygen on sphalerite-bearing materials

N.J. Welham and N. Setoudeh
Mineral Processing and Extractive Metallurgy Review, Vol.114(2), pp.65-69
2005
url
Link to Published Version *Subscription may be requiredView

Abstract

A sphalerite concentrate and two flotation rougher tails have been milled in an oxygen atmosphere for up to 10 h. Pressure measurements on the mills indicated that the concentrate had an induction time of < 2 h before significant reaction occurred whereas one of the tailings showed reaction within 1 h. The second tailings sample showed a slow pressure loss with time. All three samples showed a similar rate of pressure loss between 2 h and 10 h of milling indicating they were probably all reacting at a similar rate. Leaching of the milled powders in water showed significant increases which coincided with the pressure drops indicating that the oxidation products were water soluble; similar increases were also evident in acid.

Details

Metrics

38 Record Views
Logo image